Phosphoric acid as metal pretreatment
(→Reasons for not using phosphoric acid) |
(→Published epoxy primer and paint manufacturers' positions on the use of phosphoric acid pretreatments) |
||
Line 28: | Line 28: | ||
==Published epoxy primer and paint manufacturers' positions on the use of phosphoric acid pretreatments== | ==Published epoxy primer and paint manufacturers' positions on the use of phosphoric acid pretreatments== | ||
− | + | ===Southern Polyurethanes, Inc.=== | |
+ | *[http://www.southernpolyurethanes.com/tech%20sheets%20new/epOXY%202006.pdf Southern Polyurethanes]: | ||
+ | <blockquote> | ||
+ | ''"NEVER use SPI Epoxy over a Soda Blasted vehicle, Acid Etch/Wash Primer, Rust Converter or other Metal Treatments. NEVER!"'' | ||
+ | </blockquote> | ||
+ | |||
+ | The owner of Southern Polyurethanes has detailed some options that '''should''' solve the phosphoric acid film problem, in [http://www.hotrodders.com/forum/ospho-factory-response-173513.html#post1235021 this post on the Hotrodders Bulletin Board]. | ||
==Use of phosphoric acid in an industrial setting== | ==Use of phosphoric acid in an industrial setting== |