==Reasons for using phosphoric acid==
 
==Reasons for using phosphoric acid==
 
*Inexpensive.
 
*Inexpensive.
*[[Media blasting]] has its own set of drawbacks.for instance when done by an amiture can warp panels easily not to mention the health hazords and mess..should only be done by qualified professionals under proper conditions as far as sheetmetal goes...
+
*[[Media blasting]] has its own set of drawbacks, especially when done by a hobbyist or amateur: panel warpage, health hazards for certain media, and mess.
 
*If used perfectly, it works perfectly.
 
*If used perfectly, it works perfectly.
* no experiance is needed just reading skills(directions)and Protects bare metal from surface rust..
+
*No experience is needed; easy for amateurs to use.
 +
*Protects bare metal from surface rust.
  
 
==Reasons for not using phosphoric acid==
 
==Reasons for not using phosphoric acid==