Phosphoric acid as metal pretreatment
(→House of Kolor) |
(→House of Kolor) |
||
Line 61: | Line 61: | ||
<blockquote> | <blockquote> | ||
''"'''NOTE:''' Do not use any acid base products such as self etching primer, etc. under the KP2CF primer. This will almost certainly cause an adhesion problem. | ''"'''NOTE:''' Do not use any acid base products such as self etching primer, etc. under the KP2CF primer. This will almost certainly cause an adhesion problem. | ||
− | + | ||
− | '''NOTE:''' If you find it necessary to use a metal conditioner to remove rust, etc., be sure to thoroughly clean and neutralize the treated area following the conditioner manufacturers recommendations, then using our KC20 post sanding cleaner with a maroon scuff pad to insure all acid residue has been removed before priming. If not, this will almost certainly cause an adhesion problem."'' | + | |
+ | '''''NOTE:''' If you find it necessary to use a metal conditioner to remove rust, etc., be sure to thoroughly clean and neutralize the treated area following the conditioner manufacturers recommendations, then using our KC20 post sanding cleaner with a maroon scuff pad to insure all acid residue has been removed before priming. If not, this will almost certainly cause an adhesion problem."'' | ||
</blockquote> | </blockquote> | ||