#Scrub metal to a clean, bright finish. Wipe dry with paper towels, and let flash dry completely.
 
#Scrub metal to a clean, bright finish. Wipe dry with paper towels, and let flash dry completely.
 
#Scuff dry panel with dry scuff pad, wipe with wax and grease remover until clean and dry; when wiped with a clean towel, it comes back up clean.
 
#Scuff dry panel with dry scuff pad, wipe with wax and grease remover until clean and dry; when wiped with a clean towel, it comes back up clean.
 +
 +
 +
===Treating light body rust (from storing panels) prior to epoxy===
 +
Sand with 80 grit, wash with wax and grease remover. Use waterborne wax and grease remover, instead of solvent-borne (research exactly what that means), let set 15-30 minutes. Dry with a blower and a tack rag. Spray epoxy.
  
 