Rust
(→Muriatic acid is another name for hydrochloric acid) |
(→Rust pitting) |
||
Line 204: | Line 204: | ||
Heat the pitted area until it glows, and then cool it with oil on a rag. Clean with wax/grease remover, scuff, prime, paint. Just for small areas, because it causes wrinkles and shrink marks. | Heat the pitted area until it glows, and then cool it with oil on a rag. Clean with wax/grease remover, scuff, prime, paint. Just for small areas, because it causes wrinkles and shrink marks. | ||
+ | |||
+ | Rust pinholes are hard to repair with a welder because the "holes" are actually "craters". The hole is the bottom of a craterlike thinned out area of metal. | ||
===Removing surface rust=== | ===Removing surface rust=== |