Rust
m (→Miscellaneous (need to be sorted)) |
(→Fiberglass resin patches) |
||
Line 490: | Line 490: | ||
==Fiberglass resin patches== | ==Fiberglass resin patches== | ||
One technique that has been recommended is to grind/clean the rust, tape the underside of the panel to be patched, and then fill the holes with fiberglass resin, then paint and undercoat. This trick is not really a good idea -- when the body flexes, there will be cracks in the fiberglass pieces. Metal also expands at different rates than [[Fiberglassing|fiberglass]], causing cracks to form, allowing more rust to form in these cracks. | One technique that has been recommended is to grind/clean the rust, tape the underside of the panel to be patched, and then fill the holes with fiberglass resin, then paint and undercoat. This trick is not really a good idea -- when the body flexes, there will be cracks in the fiberglass pieces. Metal also expands at different rates than [[Fiberglassing|fiberglass]], causing cracks to form, allowing more rust to form in these cracks. | ||
+ | |||
+ | Using POR-15 (a moisture-cured urethane) and fiberglass cloth will produce a low-cost repair that will bond and flex with the metal. In fact, POR-15 sells a $20 kit to do this very thing. While this method does fill the holes and provides a rust-resistant repair, it does not restore any mechanical strength to the metal like an actual metal patch panel would. | ||
==Do metal etches leave coating?== | ==Do metal etches leave coating?== |