*Heat the pitted area until it glows, then cool it with oil on a rag. This fix should only be used on small areas because it can warp the surrounding metal, causing wrinkles and shrink marks. ''(confirm that this is acceptable practice, sounds borderline)''((I would use this method only if you are good with a hammer and dolly))
+
*Heat the pitted area until it glows, then cool it with oil on a rag. This fix should only be used on small areas because it can warp the surrounding metal, causing wrinkles and shrink marks. ''(confirm that this is acceptable practice, sounds borderline)''
  
 