Rust
(→Plasma spray welding) |
(→Rust pitting) |
||
Line 73: | Line 73: | ||
===Rust pitting=== | ===Rust pitting=== | ||
After removing all surface rust, treat with metal prep, wash, dry, sand, prime, fill the pits with polyester putty, then smooth and prime again. | After removing all surface rust, treat with metal prep, wash, dry, sand, prime, fill the pits with polyester putty, then smooth and prime again. | ||
+ | |||
+ | A spot blaster is useful for this. | ||
Or, repeatedly prime with a high build primer and block sand. You may have to prime/block several times to get the pitted area up to the same level as the surface around it. | Or, repeatedly prime with a high build primer and block sand. You may have to prime/block several times to get the pitted area up to the same level as the surface around it. | ||
+ | |||
+ | ===Removing surface rust=== | ||
*To remove surface rust, use naval jelly and steel wool. | *To remove surface rust, use naval jelly and steel wool. |