===Soda blasting issues===
 +
When soda blasting body panels, the resultant film can negatively affect finish adhesion. Epoxy primer can peel off. Soda blast medium must be "neutralized". 24 or 36 grit grinder, followed by warm water with soap. Do this with a scuff pad, and rinse thoroughly.
 +
 +
Some finish companies specifically advise against the use of their products on soda-blasted finishes.
  
 
===Penny trick for filling holes===
 
===Penny trick for filling holes===

Revision as of 10:06, 23 June 2007

Personal tools
Namespaces
Variants
Actions
Navigation
Categories
Toolbox